Ideal Hardware Products Performance
Plating Performance
Feature Test Standard Exposure (hours) Criteria
Salt Spray ASTM B117 250 No Blisters>8
ASTM D1654
Acid Salt* ASTM D714 1000 No Blisters>8
UVCON ASTM G154-00 cycle 1 1000 No fading, discoloration or rub off
D4587-91
D4329-92
G151-97
Humidity 100% Relative Humidity 1000 No blistering, discoloration or staining
Room Temperature
Ozone ASTM D1149 Vol 9.01 100 No permanent damage to film
No discoloration or softening
*Acid Salt requirements apply only to parts with PVD finish
Hardware Operation Feature
All hardware assemblies must pass a full range of motion operational test of 100,000 cycles.
(Reference ANSI / BHMA A156.2-2003, Section 9)
Hardware Strength Tests are conducted as per ANSI/BHMA A156.2-2003, Per Section 10.4), ASTM F476, Static Bolt Load Test, ANSI/BHMA A156.2-2003, Section 9.5).